Abstract:
Thermal stresses normally associated with brazing are alleviated by a low temperature brazing technique of the present invention. A low-temperature brazing paste, preferably suitable to be melted at temperatures of no greater than 200. degree. C. (e. g. , 100-200. degree. C. ), containing nanoscale (. ltoreq. 100 nanometer) size particles of gold, cadmium, copper, zinc, tin, lead, silver, silicon, chromium, cobalt, antimony, bismuth, aluminum, iron, magnesium, nitrogen, carbon, boron, and alloys and composites of these materials, is applied as a bead or as a powder spray at the junction of two components desired to be joined together. Energy from a source such as a laser beam (for example a CO. sub. 2 laser, an Nd-Yag laser or an excimer laser), flame, arc, plasma, or the like, is "walked" along the brazing material. The energy beam is sufficient to cause melting and re-crystallization of the nanoscale-particle-containing brazing paste.